US 7,579,114 B2
Method of preparing positive electrode active material
Tsutomu Ohzuku, Nara (Japan); Hiroshi Yoshizawa, Osaka (Japan); and Masatoshi Nagayama, Osaka (Japan)
Assigned to Panasonic Corporation, Osaka (Japan); and Osaka City University, Osaka (Japan)
Filed on Sep. 14, 2006, as Appl. No. 11/531,887.
Application 11/531887 is a division of application No. 10/242052, filed on Sep. 12, 2002.
Claims priority of application No. 2001-278536 (JP), filed on Sep. 13, 2001.
Prior Publication US 2007/0009424 A1, Jan. 11, 2007
Int. Cl. H01M 4/04 (2006.01); H01M 4/50 (2006.01); H01M 4/52 (2006.01)
U.S. Cl. 429—231.1  [29/623.1; 429/223; 429/224; 429/231.3; 429/221] 8 Claims
OG exemplary drawing
 
1. A production method of a positive electrode active material for a non-aqueous electrolyte battery, comprising the steps of:
introducing into a reaction vessel an alkaline solution and an aqueous solution containing two or more transition metal salts or two or more aqueous solutions containing different transition metal salts;
coprecipitating using a reductant or an inert gas to obtain a hydroxide or an oxide precursor of at least two transition metals;
drying said hydroxide or oxide at 300 to 500° C. to obtain a dry precursor; and
baking a mixture of said dry precursor and a lithium compound at a temperature of 900° C. to 1200° C. to obtain a lithium-containing transition metal oxide, wherein the lithium-containing transition metal oxide contains Mn and Ni in a 1:1 molar ratio.